Sorun Belirtisi
Sharkskin not eliminated immediately after adding PPA.
Neden Analizi
PPA takes effect only after forming a coating on the die wall; the addition amount and dispersion state affect the onset time.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience.
Çözüm
①Record the onset time to establish a benchmark; ②ensure uniform PPA dispersion; ③initially appropriately increase the addition amount; ④evaluate masterbatch carrier compatibility.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Temel Çıkarım
PPA onset requires a coating formation process; only standardized use can give the best effect.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
LLDPE; film; PPA; onset time; coating; dispersion