Processing Machinery
8 görüntüleme
LLDPE color change cleaning
Sorun Belirtisi
Prolonged color mixing after color change of LLDPE film
Neden Analizi
High melt viscosity causes slow purging; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Çözüm
Schedule production from light to dark; purge with cleaning compound; disassemble and clean the die; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
Color change relies on production scheduling plus disassembly and cleaning; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu