Molding Process 8 görüntüleme

PA12 Long-flow Thin-wall Part Temperature Strategy

Sorun Belirtisi
【Problem phenomenon】PA12 long-flow thin-wall parts had short shots at the end and could not be filled within the conventional temperature window
Neden Analizi
Long-flow low-wall-thickness products are allowed to work at the upper limit of melt temperature (up to 300℃) in exchange for fluidity, especially reinforced grades; but this must be matched with short residence time to prevent degradation
Çözüm
For long-flow thin-wall parts, take the melt temperature at the upper limit of the window up to 300℃ and shorten the residence time; cooperate with high-speed injection and mold temperature increase; perform strength verification on the first article to confirm no degradation
Temel Çıkarım
Long-flow thin-wall parts can use the 300℃ upper limit in exchange for flow, and the residence time must be shortened simultaneously; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
long flowthin walltemperature upper limitresidence time