PA6 Nozzle Solidification Clogging

Sorun Belirtisi
After a short stop, the nozzle was clogged and no material came out, making startup difficult.
Neden Analizi
PA6 crystallizes quickly and solidifies as soon as the nozzle temperature is slightly low; the nozzle heater band is faulty or heat dissipates quickly in contact with the mold; the high crystallinity of PA6 makes the nozzle a weak point.
Çözüm
①Check whether the nozzle heater band and thermocouple are normal;②appropriately increase the nozzle temperature;③shorten the mold-open residence time to reduce nozzle cooling;④enlarge the nozzle aperture when necessary;⑤empty the barrel or lower the temperature for heat preservation before stopping.
Temel Çıkarım
PA6 nozzle clogging = 'fast solidification + weak heating': the nozzle heating system is the lifeline; nylon crystallizes quickly and clogs as soon as it stops, and the heater band status and shutdown management must be in place.
PA6; nozzle clogging; solidification; heater band; aperture