Injection Molding
7 görüntüleme
PA6 '2079851475616104452 Ejection Whitening
Sorun Belirtisi
Whitening at ejector pins, obvious on dark parts.
Neden Analizi
Large gripping force, concentrated stress, insufficient cooling; PA6 crystallization shrinkage causes large gripping force on the core; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Çözüm
①Extend cooling time so that the product is fully set before demolding;②large ejection area;③appropriately reduce holding pressure to reduce gripping force and frozen internal stress;④polish the core;⑤optimize the ejector pin layout.
Temel Çıkarım
PA6 ejection whitening = 'concentrated stress': disperse ejection force and give sufficient cooling; crystalline nylon has large gripping force, and the ejection system must leave sufficient margin; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu