Material Drying
5 görüntüleme
PA66 recycled '2079851475616104451
Sorun Belirtisi
PA66 products blended with recycled material have obviously more bubble and strength problems than virgin material
Neden Analizi
Recycled material exposed in storage absorbs moisture deeply and has undergone multiple heat histories, moisture content and degradation degree both higher than new material; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Çözüm
Recycled material dried separately with time extended to 6 hours; blending ratio not over 25%; sealed storage after crushing and used as soon as possible; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
Recycled material needs separate intensified drying and limited blending; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!