Molding Process
5 görüntüleme
PA66 glass fiber reinforced warpage
Sorun Belirtisi
Glass fiber reinforced PA66 parts have warpage out of tolerance, poor flatness, and assembly datum offset
Neden Analizi
Glass fiber orientation makes PA66-GF30 flow-direction shrinkage 0.4-0.8% and transverse difference 0.2-0.4%, anisotropy causes warpage; uneven fiber distribution further amplifies deformation
Çözüm
①Gate position makes fibers uniformly oriented along the main direction; ②Mold temperature homogenization ±2℃, conformal water circuits; ③Flat parts with straightening fixtures set for 24 hours reduce warpage by 40-60%
Temel Çıkarım
Glass fiber PA66 warpage originates from orientation anisotropy; gate design, uniform-temperature cooling, and straightening fixtures constitute a complete warpage reduction solution; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu