Injection Molding
7 görüntüleme
PA66 injection pressure window
Sorun Belirtisi
Insufficient pressure causes short shots, excessive pressure causes flash and mold expansion, and fluctuation is large within the 75-125MPa window
Neden Analizi
PA66 injection pressure is conventionally 75-125MPa, and glass fiber reinforced grades need to be increased by 20-30%; material batch, wall thickness, and flow length changes all change pressure demand, and fixed parameters cannot cover all
Çözüm
①Trial-mold and finalize within 75-125MPa according to product structure; ②Set reinforced grades at the upper limit; ③Use pressure-controlled transfer point for switchover to holding; after adjustment, take continuous samples to verify the effect, confirm stability before resuming mass production
Temel Çıkarım
PA66 pressure setting should be tailored to the part; trial-mold finalization plus scientific transfer points adapt to fluctuations better than empirical parameters; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!