Material Drying
5 görüntüleme
PBAT '2079851475616104452 silver streaks and bubbles
Sorun Belirtisi
PBAT injection molded products have surface silver streaks and internal bubbles, caused by insufficient drying or degradation gas generation from excessive temperature.
Neden Analizi
PBAT has strong moisture absorption and drying is not thorough; barrel temperature too high causes thermal decomposition; screw back pressure too low mixes in air; injection speed too fast traps air; mold venting is poor.
Çözüm
①Fully dry to control moisture content; ②set barrel temperature according to manufacturer standards; ③appropriately increase back pressure; ④segmented control of injection speed; ⑤optimize mold venting.
Temel Çıkarım
Drying and temperature are the main causes of gas defects in PBAT '2079851475616104452; segmented injection is the standard anti-air-trap technology; venting design cannot be omitted.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!