Processing Machinery
4 görüntüleme
PBT product vacuum voids
Sorun Belirtisi
Vacuum holes inside thick walls.
Neden Analizi
The surface layer solidifies first and internal feeding is interrupted; holding pressure cannot penetrate.; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first when troubleshooting
Çözüm
①Core out thick areas; ②extend holding pressure; ③reduce mold temperature gradient; ④evaluate structural modification.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
Vacuum voids are a structural feeding problem.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu