Processing Machinery 4 görüntüleme

PC/ABS heat resistance deformation

Sorun Belirtisi
Deformation in high-temperature environment.
Neden Analizi
Service temperature exceeds the heat deflection temperature of the material; internal stress reduces actual heat resistance.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Çözüm
①Select heat-resistant grade; ②reduce internal stress; ③evaluate service temperature; ④heat deflection test.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
Heat resistance management relies on material selection and stress control.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
PC/ABS;heat resistance;deformation;heat deflection temperature;internal stress;material selection