Injection Molding 7 görüntüleme

PCABS injection pressure range

Sorun Belirtisi
【Problem Phenomenon】PC/ABS filling pressure set improperly, short shots and flash alternate
Neden Analizi
Injection pressure 80-140MPa (some data 80-130MPa): take the upper limit for thin-wall complex parts, the middle value for conventional parts; the PC component has high viscosity, and the pressure requirement is higher than pure ABS
Çözüm
Set within the 80-140MPa window; take the upper limit for thin walls; after filling is satisfied, gradually reduce pressure to reduce internal stress; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
PC/ABS injection 80-140MPa, thin walls take the upper limit; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
injection pressureshort shotthin wallinternal stress