Material Drying 5 görüntüleme

Delamination of PE Film Lamination

Sorun Belirtisi
After dry lamination of PE film, peel strength is low, tunnel effect or delamination occurs, and the laminated product is scrapped.
Neden Analizi
Excessive exudation of slip agent on the film surface hinders adhesive wetting; excessive or insufficient corona treatment, film surface contamination, and improper adhesive ratio and curing all cause insufficient bonding force at the lamination interface.
Çözüm
①Select a low-slip/low-exudation system for lamination film; ②Control the corona degree (meeting the standard is enough, do not overdo it); ③Clean the film surface; ④Standardize the adhesive mixing ratio and curing process; ⑤Carry out peel strength sampling inspection and retain samples.
Temel Çıkarım