Menü
Malzemeler Makineler
İçgörüler
Makaleler Videolar Sorun ve Çözüm
About
Chembull Hakkında Medya Ortakları
Bize Ulaşın
Dil
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Sorun ve Çözüme Geri Dön
Extrusion & Post 11 görüntüleme

PET Bottle Transfer Interval Too Long

Sorun Belirtisi
The interval from heating to the blowing station is long for the preform, and pearlescent streaks appear on the bottle body.
Neden Analizi
The preform cools naturally after leaving the oven, the surface undergoes secondary crystallization and the internal-external temperature difference increases, forming pearlescence during stretching; the standard requires the transfer interval to be controlled within 2 seconds.
Çözüm
①Optimize the robot/turntable cycle to make transfer <2 seconds; ②reduce waiting after the oven; ③check equipment linkage timing.
Temel Çıkarım
From preform leaving the oven to blowing = a race against 2 seconds.
PET; bottle blowing; transfer time; secondary crystallization; pearlescence

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI