Material Drying 8 görüntüleme

PET Bottle Body White Haze (Hydrolysis Type)

Sorun Belirtisi
The whole bottle presents uniform hazy turbidity, accompanied by brittleness and rough surface, tiny bubbles visible in severe cases, and strength significantly decreased.
Neden Analizi
The preform is damped during storage or insufficiently dried; during blowing heating, moisture triggers hydrolysis, molecular chains break and micropores are produced that scatter light; preforms stored too long in high-humidity environments are a high-incidence scenario.
Çözüm
①Store preforms sealed and control warehouse humidity; ②re-dry damped preforms or switch to fresh preforms; ③test preform moisture content and IV value; ④first-in first-out to shorten the inventory cycle.
Temel Çıkarım
Hydrolysis-type white haze is often accompanied by embrittlement and is a material defect rather than a pure process problem; controlling moisture from the preform storage stage is the most economical, and damped preforms are not recommended to go online directly.
PET; bottle blowing; white haze; hydrolysis; damped; storage