Material Drying 4 görüntüleme

PET dried material anti-re-moistening

Sorun Belirtisi
PET chips that passed drying show white haze defects again after being stored in the silo for half a day
Neden Analizi
PET chips absorb moisture quickly, and dried material exposed to a high-humidity environment re-moistens rapidly, with the previous efforts wasted during storage; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Çözüm
Keep the dried material silo under positive pressure of dry air and sealed; storage does not exceed 4 hours; conveying uses a closed-loop dry air system; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
PET dried material is kept sealed and dry throughout, and exposure means failure; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems