PET zipper monofilament
Sorun Belirtisi
Insufficient strength of zipper PET monofilament after tooth forming
Neden Analizi
Monofilament orientation and crystallinity affect the engagement strength after tooth forming; the process window is narrow; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Çözüm
Optimize monofilament draw ratio and heat setting; control tooth forming temperature; test according to zipper industry standards; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
Zipper monofilament controls strength and formability according to industry standards; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!