PPO Injection Speed Grading

Sorun Belirtisi
【Problem Phenomenon】PPO injection speed is set improperly, and jetting and short shot problems alternate
Neden Analizi
SABIC recommends injection speed from medium to fast; too slow means front freezing and short shots, too fast means shear and jetting risks; long-runner thin walls need fast speed but must be matched with venting
Çözüm
Set injection speed in grades from medium to fast; fast speed for long-runner parts matched with venting; reduce initial speed when jetting signs appear; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Temel Çıkarım
PPO injection medium to fast; between fast and slow depends on flow length and venting; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems