PP Flow Mark

Sorun Belirtisi
【Problem Phenomenon】Wavy flow marks on PP surface
Neden Analizi
The cold solidified film at the front breaks; low mold temperature and slow injection speed; PP rapid solidification aggravates it; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Çözüm
Increase mold temperature and melt temperature; multi-stage injection optimization; enlarge runners and gates; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
For PP flow marks increase temperature and stabilize speed, rapid solidification is the internal cause; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future