Injection Molding
5 görüntüleme
HIPS Product Surface Orange Peel
Sorun Belirtisi
The product surface shows orange-peel-like microscopic unevenness.
Neden Analizi
Low mold temperature causes poor replication or injection speed is slow; the rubber phase in HIPS also makes the surface state more sensitive to the process.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Çözüm
①Increase mold temperature; ②increase injection speed; ③improve cavity polishing; ④appropriately increase material temperature.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
HIPS surface quality is guaranteed by temperature and speed; high gloss requirements need to be matched with mold polishing.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu