Menü
Malzemeler Makineler
İçgörüler
Makaleler Videolar Sorun ve Çözüm
About
Chembull Hakkında Medya Ortakları
Bize Ulaşın
Dil
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Sorun ve Çözüme Geri Dön
Material Analysis 12 görüntüleme

PVC Profile Low Weld Corner Strength

Sorun Belirtisi
After welding of door and window profiles, weld corner strength is insufficient, corners crack, and the whole window's air-tightness, water-tightness and safety are affected.
Neden Analizi
Poor plasticization degree, too high filler in formula or improper welding process (temperature/pressure/time) cause insufficient molecular entanglement at the welding interface; poorly plasticized profiles are 'congenitally deficient', no matter how good the welding is, the strength cannot be made up.
Çözüm
①Verify the gelation degree of the mixture, ensure plasticization; ②Optimize the three welding elements (temperature/pressure/time); ③Control filler and regrind proportion; ④Use formula materials with qualified strength; ⑤Regularly test weld corner strength.
Temel Çıkarım
PVC weld corner strength = 'plasticization quality + welding process': plasticization is the foundation, welding is the surface; poorly plasticized material cannot be welded firmly no matter what — ensure plasticization first, then talk about welding parameters.
PVC; profile; weld corner strength; welding; plasticization