Extrusion & Post 12 görüntüleme

PVC Profile Surface Streaks

Sorun Belirtisi
Longitudinal light-dark streaks on profile surface, affecting appearance consistency, more obvious on co-extruded profiles.
Neden Analizi
Periodic shedding of die buildup/exudates, die damage or uneven plasticization; unstable co-extrusion layer interface also shows streaks; streaks are the external manifestation of die condition and melt uniformity.
Çözüm
①Clean die buildup and foreign matter; ②Repair and polish die damaged areas; ③Improve plasticization quality, eliminate unplasticized particles; ④Check parameter matching of co-extrusion layers; ⑤Stabilize extrusion temperature and pressure.
Temel Çıkarım
PVC streaks = 'die condition + plasticization uniformity': buildup shedding, die damage, poor plasticization are the three sources; the regularity of streaks can infer whether it is periodic buildup or persistent damage.
PVC; profile; streak; die; plasticization