Thermoforming
5 görüntüleme
PVC '2079851475616104458 Discoloration and Burning
Sorun Belirtisi
PVC sheet '2079851475616104458 shows yellow/brown streaks, sour odor, products scrapped.
Neden Analizi
De-HCl occurs when temperature exceeds 170~200℃; local hot spots of heaters, too long heating time; PVC '2079851475616104458 temperature red line is exactly the degradation temperature.
Çözüm
①Reduce oven temperature to safe window; ②Check whether ceramic heaters have local hot spots; ③Shorten heating cycle, avoid long-time heating; ④Strengthen workshop ventilation to exhaust decomposition gas; ⑤Use temperature measurement means to monitor actual sheet temperature.
Temel Çıkarım
PVC '2079851475616104458 'temperature red line = degradation temperature': local hot spots are invisible killers; PVC '2079851475616104458 must precisely control temperature within the window — hot spots and overtime both trigger de-HCl.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu