PVC Rigid Pipe Insufficient Impact Resistance
Sorun Belirtisi
PVC water supply pipe low-temperature falling weight impact unqualified, brittle fracture.
Neden Analizi
Poor plasticization, insufficient or poorly dispersed impact modifier, too much regrind; plasticization and modification system jointly determine impact resistance; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience.
Çözüm
①Verify plasticization degree (e.g. dichloromethane immersion method); ②Ensure impact modifier fully dispersed; ③Control regrind proportion and re-dry; ④Do low-temperature falling weight impact sampling test to verify impact performance; ⑤Optimize formula system (additives, fillers, modifiers).
Temel Çıkarım
PVC rigid pipe impact resistance = 'plasticization + modification system': poor plasticization and insufficient modifier are the two roots; low-temperature impact is the hard indicator of rigid pipe, plasticization and formula must both reach standard.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!