Processing Machinery
5 görüntüleme
TPE Barrel Temperature Zoning
Sorun Belirtisi
TPE plasticization is uneven and the melt fluctuates
Neden Analizi
The barrel temperature gradient is unreasonable; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Çözüm
Barrel gradient: rear zone 160℃, middle zone 185℃, front zone 205℃; back pressure at the lower limit; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
The TPE temperature gradient is gentle and the back pressure is low; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!