Processing Machinery
6 görüntüleme
TPE Nozzle Temperature
Sorun Belirtisi
TPE nozzle drooling
Neden Analizi
Low melt viscosity makes drooling easy; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Çözüm
Match nozzle temperature; suck back; needle valve nozzle; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
Drooling relies on suck back and structure; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu