TPE Transparent Material Temperature

Sorun Belirtisi
The haze of transparent TPE products exceeds the standard
Neden Analizi
Improper temperature causes phase separation affecting transparency; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Çözüm
Transparent TPE follows the supplier's temperature window; uniform melt temperature; mold temperature optimization; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
Transparent TPE has a narrower temperature window; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
TPE transparency haze temperature