Processing Machinery 5 görüntüleme

TPE short shot

Sorun Belirtisi
TPE thin-walled parts are underfilled
Neden Analizi
High melt viscosity causes large filling resistance; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Çözüm
Take the upper limit of melt temperature; increase speed; enlarge the gate; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Temel Çıkarım
Short shot relies on temperature, speed, and gate; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later