Extrusion & Post
10 görüntüleme
EEA extrusion die drool and carbon deposits
Sorun Belirtisi
After EEA extrusion shutdown, brown carbon deposit layer found on the die inner wall, black specks on the product surface after restarting
Neden Analizi
EEA heated for a long time in the die residence zone, oxidized, decomposed and carbonized; die not cleaned in time during shutdown; extrusion temperature too high accelerating carbonization
Çözüm
1) Flush the die with pure PE for 3-5min before shutdown to remove EEA residue; 2) Disassemble and clean the die immediately after shutdown; 3) Reduce extrusion temperature by 5-10°C to reduce carbonization tendency; 4) Optimize die runners to reduce dead zones in the residence zone
Temel Çıkarım
Die carbon deposits are caused by thermal oxidation and untimely cleaning; PE flushing and timely cleaning are the key