Injection Molding 6 görüntüleme

EEA Obvious Surface Color Difference

Sorun Belirtisi
Different parts of EEA products have different color shades, color difference ΔE>5
Neden Analizi
Uneven dispersion of color masterbatch; pigment orientation during injection causes uneven color distribution; barrel temperature fluctuation causes color change
Çözüm
1) Use the masterbatch method for color masterbatch to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature within ±2°C
Temel Çıkarım
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
EEA color difference color masterbatch dispersion pigment orientation temperature stability