EEA Insufficient Low-Temperature Performance
Sorun Belirtisi
EEA product impact strength at -40°C is below application requirements
Neden Analizi
EEA ethyl acrylate content is low, leading to insufficient low-temperature toughness
Çözüm
1) Select high EA content EEA with EA>18% to improve low-temperature toughness; 2) Add 5wt% EEA elastomer for toughening; 3) Anneal to release orientation stress
Temel Çıkarım
EEA low-temperature performance is determined by EA content; selecting a high EA grade is fundamental