Injection Molding
6 görüntüleme
EMA '2079851475616104452 Demolding Difficulty
Sorun Belirtisi
EMA injection molded products have large demolding force, product deformation or scratch damage, demolding time accounts for 30% of the cycle
Neden Analizi
Large adhesion between EMA and mold cavity; insufficient draft angle <0.5°; insufficient cooling time, product demolded before fully solidified; ejection mechanism design unreasonable
Çözüm
1) Increase mold draft angle to 1-2°; 2) Extend cooling time so the product is fully solidified before demolding; 3) Polish mold surface to Ra<0.2μm; 4) Increase ejection area, use a large-area ejector plate; 5) Spray mold release agent (temporary solution)
Temel Çıkarım
Demolding difficulty is caused by adhesion and insufficient mold design; increasing draft angle is the fundamental measure