Processing Machinery 5 görüntüleme

Poor EMA plasticization

Sorun Belirtisi
Unmelted particles appear in EMA products with incomplete plasticization
Neden Analizi
Screw compression ratio insufficient <2.5 with low plasticizing pressure; screw speed too low with insufficient shear; processing temperature too low
Çözüm
1) Select screw with compression ratio >3; 2) Increase screw speed to increase shear; 3) Increase processing temperature by 5-10°C
Temel Çıkarım
Poor plasticization is caused by improper screw design; optimizing screw and raising temperature are key