Molding Process 8 görüntüleme

EVA foam shrinkage is large

Sorun Belirtisi
EVA foamed shoe sole 24h shrinkage >5%
Neden Analizi
Cell gas diffuses out causing shrinkage; crosslinking <60% with poor recovery aggravates shrinkage
Çözüm
1) Increase DCP to 0.5-0.8wt% with crosslinking >60%; 2) Reduce foaming temperature by 5-10°C; 3) 80°C/1h post-treatment; 4) VA18-28% moderate
Temel Çıkarım
EVA foam shrinkage is caused by gas diffusion and insufficient crosslinking; increasing crosslinking degree is key
EVA foam shrinkage crosslinking degree DCP post-treatment VA content