Molding Process 6 görüntüleme

EVA foam locally unfoamed

Sorun Belirtisi
EVA foamed shoe material has local hard lumps with density >0.5g/cm³
Neden Analizi
Blowing agent AC locally undecomposed due to insufficient temperature; DCP locally excessive with premature crosslinking suppressing expansion
Çözüm
1) Mold temperature ±2°C to ensure global decomposition; 2) DCP masterbatch method to ensure uniform crosslinking; 3) AC masterbatch method to ensure dispersion
Temel Çıkarım
Local unfoamed areas are caused by insufficient temperature and uneven crosslinking; uniform temperature control and masterbatch method are key
EVA foam local unfoamed blowing agent dispersion mold temperature control uniform crosslinking