Processing Machinery 5 görüntüleme

EVA film heat-sealing window is narrow

Sorun Belirtisi
EVA heat-sealing window only 5°C, 125-130°C, unstable
Neden Analizi
High VA content with low melting temperature and narrow window; equipment temperature control ±3°C exceeding
Çözüm
1) VA15-18% moderate, widening to 10°C; 2) Temperature control ±1°C; 3) Film ±5%; 4) Reduce speed to increase contact time
Temel Çıkarım
Narrow EVA heat-sealing window is caused by high VA; moderate VA and precise temperature control are key
EVA film heat-sealing window VA content temperature control accuracy heat-sealing speed