Processing Machinery 5 görüntüleme

EVA poor plasticization

Sorun Belirtisi
Unmelted particles appear in EVA products with incomplete plasticization
Neden Analizi
Insufficient screw compression ratio <2.5 with low plasticizing pressure; screw rotation speed too low with insufficient shear; processing temperature too low
Çözüm
1) Select a screw with compression ratio >3; 2) Increase screw rotation speed to increase shear; 3) Increase processing temperature by 5-10°C
Temel Çıkarım
Poor plasticization is caused by improper screw design; optimizing the screw and increasing temperature are key
EVA poor plasticization screw compression ratio shear rate processing temperature