Material Analysis 12 görüntüleme

EVOH product dimensional change during long-term storage

Sorun Belirtisi
EVOH product dimensions change ±2-3% after 3 months of storage, exceeding the ±0.5% requirement
Neden Analizi
EVOH physical aging relaxation causing continuous dimensional change; secondary crystallization slowly changing density and dimensions; slow migration of low molecular substances changing local density
Çözüm
1) Annealing treatment at 80°C/4h before product shipment to stabilize dimensions; 2) Select high molecular weight grades to reduce low molecular substances; 3) Slight crosslinking to reduce molecular chain mobility and suppress aging; 4) Control storage environment temperature at 23±2°C to reduce temperature change effects
Temel Çıkarım
Dimensional change is caused by physical aging; annealing treatment and slight crosslinking are measures to stabilize dimensions
EVOH dimensional stability physical aging annealing secondary crystallization slight crosslinking