Extrusion & Post 11 görüntüleme

EVOH Surface Snakeskin Pattern

Sorun Belirtisi
EVOH extruded product surfaces show snakeskin-like irregular texture
Neden Analizi
Extrusion temperature too low, melt elastic recovery uneven; die temperature distribution uneven
Çözüm
1) Increase extrusion temperature to the processing temperature range; 2) Homogenize die temperature ±2°C; 3) Reduce extrusion rate to decrease elastic recovery
Temel Çıkarım
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed are key
EVOHsnakeskin patternextrusion temperatureelastic recoverydie temperature control

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu