Rough Surface in PU Extrusion

Sorun Belirtisi
PU extruded product surface roughness Ra>5μm, exceeding the requirement
Neden Analizi
Extrusion temperature too low <60°C, melt flow unstable; die inner wall rough or damaged; PU melt elasticity, extrusion swell uneven
Çözüm
1) Increase extrusion temperature to 60-120°C; 2) Polish die inner wall Ra<0.4μm; 3) Reduce extrusion rate by 10-15%; 4) Add 0.3-0.5wt% external lubricant
Temel Çıkarım
Surface roughness is caused by low-temperature extrusion and die defects; increasing temperature and polishing the die are the core countermeasures
PU extrusionsurface roughnessdie polishingextrusion temperaturemelt elasticity