Extrusion & Post 11 görüntüleme

Dense surface pits of PU

Sorun Belirtisi
Dense 0.1-0.3mm pits on PU product surface, affecting appearance and coating adhesion
Neden Analizi
Raw material contains impurity particles >0.05%; mold cavity surface damage or corrosion pits
Çözüm
1) Replace with pure raw material with impurities <0.01%; 2) Repair and polish mold cavity to Ra<0.2μm; 3) Filter raw material to remove particles
Temel Çıkarım
Pits are caused by raw material impurities and mold damage; pure raw material and mold maintenance are key
PU surface pits impurity particles mold repair raw material purity