Injection Molding 4 görüntüleme

Tiger skin pattern on PU surface

Sorun Belirtisi
Tiger skin pattern on PU injection molded product surface, alternating light and dark stripes 2-5mm wide
Neden Analizi
Unstable injection speed, melt front fluctuating fast and slow; mold temperature too low <30°C, front cools rapidly
Çözüm
1) Multi-stage injection slow-fast-slow to stabilize the front; 2) Increase mold temperature to 40-50°C; 3) Increase injection pressure for stable advancement
Temel Çıkarım
Tiger skin pattern is caused by unstable injection front; multi-stage injection and high mold temperature are key
PU tiger skin pattern injection speed multi-stage injection mold temperature control

Bu faydalı oldu mu?