Material Analysis
6 görüntüleme
Insufficient toughness of PU, brittle fracture
Sorun Belirtisi
PU product elongation at break <50%, brittle fracture without yielding
Neden Analizi
PU molecular weight too low, insufficient toughness foundation; excessive crosslinking, toughness lost; coarse crystallization, increased brittleness
Çözüm
1) Select high molecular weight PU to improve toughness; 2) Control crosslinking degree to avoid excess; 3) Nucleating agent to refine crystallization and improve toughness
Temel Çıkarım
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is key