PVA '2079851475616104452 flow marks
Sorun Belirtisi
PVA injection molded product surface shows radial flow marks centered on the gate
Neden Analizi
Injection speed too fast causing unstable melt front; mold temperature too low <30°C, front cools rapidly forming marks
Çözüm
1) Adopt multi-stage injection speed slow-fast-slow to control front stability; 2) Raise mold temperature to 40-50°C to delay front cooling; 3) Stabilize injection pressure to avoid fluctuation; 4) Enlarge gate area to reduce sudden pressure change at the gate
Temel Çıkarım
Flow marks are caused by unstable injection front and rapid cooling; multi-stage injection and high mold temperature are the key