Extrusion & Post 11 görüntüleme

Extruded pipe bent, not straight

Sorun Belirtisi
The extruded pipe is bent and not straight, longitudinal warpage deformation, unable to meet straightness requirements
Neden Analizi
Uneven cooling, large differences in cooling rates in all directions of the pipe Haul-off device eccentric or misaligned Extrusion temperature too high, pipe rigidity insufficient when just exiting the die Die and mandrel eccentric Uneven pipe wall thickness causing shrinkage differences
Çözüm
Improve cooling to ensure uniformity in all directions Calibrate the haul-off device to ensure alignment Appropriately reduce the extrusion temperature to the lower value of 170-230°C Adjust the concentricity of die and mandrel Control wall thickness uniformity
Temel Çıkarım
Pipe bending needs to be addressed from uniform cooling and alignment