Material Analysis 12 görüntüleme

CEF hardness too high

Sorun Belirtisi
The Shore hardness of the CEF product is 5-10 degrees higher than the target and feels hard
Neden Analizi
The CEF crystallinity is high and the rigidity increases; too much filler is added; the cooling is too fast, the crystallization is imperfect but the rigidity is frozen
Çözüm
1) Reduce the cooling rate to make the crystallization perfect and reduce the hard feel; 2) Reduce the amount of filler added; 3) Add plasticizer 0.5wt% to reduce hardness
Temel Çıkarım
High hardness is caused by crystallization and fillers; adjusting cooling and fillers is the key