Extrusion & Post 11 görüntüleme

Delamination in Blending CMC with Incompatible Resins

Sorun Belirtisi
When CMC is blended with polar resins such as PA/ABS, the extrudate completely delaminates and the mechanical properties are extremely poor
Neden Analizi
The polarity difference between CMC and polar resins is large, compatibility is zero, interfacial adhesion is extremely low, and no compatibilizer is used
Çözüm
1)Use CMC grafted compatibilizer CMC-g-MAH 2-5wt%; 2)Add epoxy compatibilizer 1-2wt%; 3)CMC addition <10wt% to keep the other resin as the continuous phase; 4)Twin-screw high-shear blending to disperse CMC to <0.3μm
Temel Çıkarım
Blends with large polarity differences require reactive compatibilizers to form chemical bonding at the interface to solve the problem
CMC blend delaminationpolarity differenceCMC-g-MAHreactive compatibilizationinterfacial bonding