Material Analysis 5 görüntüleme

DSTDP low elongation at break

Sorun Belirtisi
DSTDP product elongation at break <100%, below the 200% requirement
Neden Analizi
DSTDP molecular weight on the low side, chains short, entanglement insufficient; excessive orientation, transverse elongation extremely low; excessive crosslinking restricting chain slippage
Çözüm
1) Select high molecular weight DSTDP to increase entanglement density; 2) reduce orientation, lower injection speed; 3) control crosslinking degree to avoid excess
Temel Çıkarım
Low elongation at break is caused by low molecular weight and orientation; selecting high MW and reducing orientation are key
DSTDPelongation at breakmolecular weightorientation controlcrosslinking degree