Molding Process 8 görüntüleme

DSTDP poor antistatic effect

Sorun Belirtisi
DSTDP product surface resistance >10¹²Ω, severe static electricity
Neden Analizi
Antistatic agent addition insufficient <0.1wt%; antistatic agent migration rate slow, not reaching the surface
Çözüm
1) Increase antistatic agent to 0.3-0.5wt%; 2) select fast-migrating antistatic agent; 3) surface coat antistatic liquid for immediate effect
Temel Çıkarım
Poor antistatic effect is caused by insufficient addition; increasing antistatic agent is key
DSTDPantistaticantistatic agentsurface resistancemigration rate