Material Analysis 12 görüntüleme

Glass Fibre fast UV aging

Sorun Belirtisi
Glass Fibre after UV irradiation 48h mechanical properties drop >20%, yellowing
Neden Analizi
Glass Fibre molecular chains rapidly degrade by photo-oxidation under UV; surface molecular chains break forming microcracks
Çözüm
1) Add UV absorber 0.3-0.5wt% to block UV; 2) add HALS 0.2wt% radical scavenging; 3) carbon black 2wt% physically shields UV
Temel Çıkarım
Fast UV aging is caused by photo-oxidation; UV absorber and HALS are key
Glass FibreUV agingUV absorberHALSradical scavenging